The recommended silver content depends on the required conductivity in combination with tensile strength. We can offer you the CuAg in four different Ag contents: Ag0,1%, Ag0,2% and Ag2%. CuAg has a very high conductivity, high tensile strength, high elongation, high corrosion resistivity, high flex life, bright and shiny surface, good weldability and solderability. Lamifil can offer this alloy with a maximum of 5 ppm Oxygen.
| ELECTRICAL PROPERTIES (reference 1,8mm) | |||
|---|---|---|---|
| Minimum electrical conductivity | % IACS | 96 | |
| Average electrical conductivity | % IACS | 97 | |
| Electrical resistivity | nOhmm | 17,96 | |
| MECHANICAL PROPERTIES (reference 1,8mm) | |||
| Minimum tensile strength | MPa | 490 | |
| Average tensile strength | MPa | 510 | |
| Elongation | % | 1 | |
| PHYSICAL PROPERTIES (reference 1,8mm) | |||
| Temperature coefficient | 10-3/K | 3,77 | |
| Coefficient of thermal expansion | 10-6/K | 17,6 | |
| Density | g/cm³ | 8,89 | |
| CHEMICAL COMPOSITION (reference value) | |||
| Cu | O2 | Ag | |
| balance | < 5ppm | 0,2% | |
| Standards | |||
| Customer specific | |||
| Product information is subject to change without notice and does not represent a commitment on the part of Lamifil NV. Lamifil NV assumes no responsibility for any errors that may appear in this information. | |||