CuSn0,3 – C18835
Lamifil offers the Cu-Sn in two variants: CuSn0,3 and a CuSn0,8 with a higher resistibility and higher tensile strength. Lamifil can offer this alloy with a maximum of 5 ppm Oxygen.
| ELECTRICAL PROPERTIES (reference 1,8mm) | |||
|---|---|---|---|
| Minimum electrical conductivity | % IACS | 77 | |
| Average electrical conductivity | % IACS | 80 | |
| Electrical resistivity | nOhmm | 22,39 | |
| MECHANICAL PROPERTIES (reference 1,8mm) | |||
| Minimum tensile strength | MPa | 520 | |
| Average tensile strength | MPa | 540 | |
| Elongation | % | 1 | |
| PHYSICAL PROPERTIES (reference 1,8mm) | |||
| Temperature coefficient | 10-3/K | 3 | |
| Coefficient of thermal expansion | 10-6/K | 17,6 | |
| Density | g/cm³ | 8,92 | |
| CHEMICAL COMPOSITION (reference value) | |||
| Cu | O2 | Sn | |
| balance | < 5ppm | 0,25% | |
| Standards | |||
| CW129C | |||
| LV112-4 | |||
| EN1977 | |||
| UNS number | |||
| C18835 | |||
| Product information is subject to change without notice and does not represent a commitment on the part of Lamifil NV. Lamifil NV assumes no responsibility for any errors that may appear in this information. | |||